Temel Ferritik Çelikler
X2CrTi12 – (1.4512) / S40900 / SUS409L / Z3CT12 / 409S
Uygulama Bilgileri
Genel Kimliği
X2CrTi12 – 1.4512
| Grade | X2CrTi12 |
| Number | 1.4512 |
Eş Değer Referansları
X2CrTi12 – 1.4512
| EU – EN | X2CrTi12 |
| USA | S40900 |
| France, AFNOR | Z3CT12 |
| England, BS | 409S |
| Japan, JIS | SUS409L |
Standartlar
X2CrTi12 – 1.4512
| Standart 1 | EN 10088-2: 2005 |
| Standart 2 | EN 10296-2: 2005 |
| Standart 3 | EN 10297-2: 2005 |
| Standart 4 | EN 10088-1: 2005 |
| Standart 5 | EN 10088-4: 2009 |
Kimyasal Kompozisyonu
X2CrTi12 – 1.4512
| C | max 0.03 |
| Si | max 1.00 |
| Mn | max 1.00 |
| P | max 0.040 |
| S | max 0.015 |
| Cr | 10.5 – 12.5 |
| Ti | 0.65 |
Mekanik Özellikleri
X2CrTi12 – 1.4512
| Rm – Tensile strength (MPa) (+A) | 380 – 560 |
X2CrTi12 – 1.4512
| Rp0.2 0.2% Geçirmezlik Direnci (MPa) (+QT650) | 210 |
X2CrTi12 – 1.4512
| A – Min. elongation at fracture (%) (+A) | 25 |